Назив: Advantages of combined sintering compared to conventional sintering of mechanically activated magnesium titanate
Аутори: Filipović, Suzana
Obradovic, Nina
Pavlović, Vladimir
Kosanović, Darko
Mitric M.
Mitrovic, Nebojsa
Pouchly V.
Kachlík, Martin
Maca K.
Датум издавања: 2014
Сажетак: © 2014 Science of Sintering. In this article, the advantages of combined sintering in comparison with the conventional one, of mechanically activated magnesium titanate ceramic were investigated. The stoichiometric mixtures of MgO and TiO2 were mechano-chemically activated for 0, 10, 40, 80 and 160 minutes by ball milling and then isostatically pressed (CIP) to form green bodies. Conventional sintering was realized by heating up to 1400oC and hold for 30 minutes in air atmosphere. Resulting ceramic samples with closed porosity were post-sintered by pressure assisted technique Hot Isostatic Pressing (HIP) at 128oC/3h in argon atmosphere with a pressure of 200 MPa. The best results were observed in the case of samples post-sintered by HIP, when single-phase MgTiO3 samples with relative density of 96% were prepared.
URI: https://scidar.kg.ac.rs/handle/123456789/12466
Тип: article
DOI: 10.2298/SOS1403283F
ISSN: 0350-820X
SCOPUS: 2-s2.0-84920937736
Налази се у колекцијама:Faculty of Technical Sciences, Čačak

Број прегледа

460

Број преузимања

12

Датотеке у овој ставци:
Датотека Опис ВеличинаФормат 
PaperMissing.pdf
  Ограничен приступ
29.86 kBAdobe PDFСличица
Погледајте


Ставке на SCIDAR-у су заштићене ауторским правима, са свим правима задржаним, осим ако није другачије назначено.