Назив: Neke specifičnosti ispitivanja čeličnih bešavnih boca za ukapljene plinove
Аутори: P. Todoric
B. Grizelj
Aleksandrovic, Srbislav
Marušić V.
Датум издавања: 2012
Сажетак: Seamless steel pressure vessels for liquefied gases, are thermal treated by quenching and tempering after the formation of tubes. Tests of the mechanical properties have been conducted on specimens made from bodies and from the vessel neck. In tensile tests, curves of plastic flow of material were recorded. Intensity of hardening deformation is calculated. From the ratio of total elongation and elongation at maximum load is estimated affinity to the brittle fracture. Based on these results it was concluded that the vessel neck characteristics of strength are almost unchanged compared to the body of the vessel, increasing the minimum deformation of the devastation from 12.8% to 15.1%. It was concluded that results of the stress curve flow recording can serve as a preliminary indicator of anomalies that could contribute to unsatisfactory results of the burst test.
URI: https://scidar.kg.ac.rs/handle/123456789/20361
Тип: conferenceObject
Налази се у колекцијама:Faculty of Engineering, Kragujevac

Број прегледа

335

Број преузимања

8

Датотеке у овој ставци:
Датотека Опис ВеличинаФормат 
Plin Osijek 2012-28_1-28_12.pdf453.12 kBAdobe PDFСличица
Погледајте


Ова ставка је заштићена лиценцом Креативне заједнице Creative Commons