Please use this identifier to cite or link to this item: https://scidar.kg.ac.rs/handle/123456789/20730
Full metadata record
DC FieldValueLanguage
dc.rights.licenseAttribution-NonCommercial-NoDerivs 3.0 United States*
dc.contributor.authorArsić, Dušan-
dc.contributor.authorNikolic, Ruzica-
dc.contributor.authorLazic, Vukic-
dc.contributor.authorArsić, Aleksandra-
dc.contributor.authorSavić, Zoran-
dc.contributor.authorDjačić, Slaviša-
dc.contributor.authorHadzima, Branislav-
dc.date.accessioned2024-05-13T09:04:50Z-
dc.date.available2024-05-13T09:04:50Z-
dc.date.issued2019-
dc.identifier.citationD. Arsić, R. Nikolić, V. Lazić, A. Arsić, Z. Savić, S. Djačić, B. Hadzima, Reparatory surface welding of the fractured tooth of the bucket‐wheel excavator girth gear, 9th International Scientific Conference - IRMES 2019 - Research and Development of Mechanical Elements and Systems, Kragujevac, 2019, 5-7 September, pp. 184-185, ISBN 978‐86‐6335‐061‐8en_US
dc.identifier.isbn978‐86‐6335‐061‐8en_US
dc.identifier.urihttps://scidar.kg.ac.rs/handle/123456789/20730-
dc.description.abstractFrequent premature damages and fractures of components or the whole structure of bucket-wheel excavators at open-pit mines occur in exploitation. That is explained either by inadequate design and construction or by insufficient knowledge of the material properties, welded joints or oversights in manufacturing. Besides the direct losses due to damage or fracture of the excavator, the disruption in the power production and supply can cause significant indirect losses. The considered bucket-wheel excavator was employed for 5000 hours, when the fracture of the tooth of the girth gear, which enables the circular motion of the excavator's upper structure, occurred. The gear was made of the cast steel GS 40 MnCrSi3 V. To predict the cast steel resistance to crack propagation, the fracture parame-ters were calculated, namely the critical value of the stress intensity factor – the facture toughness KIc and the critical crack length acr, based on the obtained values of the material's impact energy and the yield stress, according to the Barsom-Rolfe model. The calculated value of the critical crack length was 61.9 mm. After the necessary calculations, the repara-tory surface welding technology of the fractured tooth has been proposed. Due to the complex construction solution of the girth gear and its function in exploitation, it was neces-sary to precisely define a large number of details and carefully consider and execute all the operations in the methodology of manufacturing the new tooth. This was an imperative in order to ensure the safety of the repaired girth gear exploitation, since the smallest over-sight, underestimate or improper execution could cause serious problems in operation of the BWE as a whole. This is the reason why the preparation procedure for the hard-facing technology is presented, as well. First, the weldability of the cast steel was determined by using various equations. According to equivalent carbon formula of the International Weld-ing Institute, for maximal value of the chemical elements composition of the GS 40 MnCrSi3 V, the limiting value for the good weldability of this material is greater than 0.45. The value obtained by the Ito-Bessyo formula also surpasses the limiting value for the good weldability of 0.30. Based on the obtained results, fact is that this steel is prone to cold cracks appear-ance, what prompted the necessity for the hard-facing of the broken tooth to be performed with preheating and controlled cooling. Also, according to formula for the Hot Cracking Sensitivity (HCS) it was established that this material is prone to appearance of the hot cracks, as well, since the obtained value for the HCS is less than 4, which is the limiting value for this type of steels with tensile strength of about 700 (MPa). After detailed investigation of weldability, the hardfacing procedure was proposed as well as all the presented prepara-tory and depositing operations. Due to the girth gear construction (dimensions and mass) and conditions of the hard-facing execution without the heat treatment, for the filling vol-ume greater than 500 (cm3), the recommended preheating temperature is within range 100 to 150 ºC. Depositing of the I layer was executed by the austenitic electrode E 18 8Mn B 22, while the II layer was deposited by the basic electrode E 1-UM-300 (DIN 8555). After the hard-facing, machining of the gears to measures defined by the coordinate measuring device was performed in accordance with clearances (tolerances) prescribed by the exca-vator manufacturer's documentation. Reparation of the girth gear tooth of the bucket wheel excavator SRs 2000×32/5.0 by the presented methodology was executed in 2013. The time gap of about 5 years, from the performed reparatory hard-facing to preparation of this paper, appeared due to the fact that the repaired girth gear's behavior was monitored in exploitation. Considering that the new tooth fractured after only a year in operation and that the repaired excavator is still in operation at the open pit mine "Kostolac" (Serbia), it could be concluded that the repara-tion was successful. It should be emphasized that in this way the large financial effect was realized since the construction of the new girth gear would cost over 500.000 €. If the time, needed for manufacturing the new girth gear, which is about 6 to 9 months, would also be included in this calculation, as well as effect of the electric power that would not be pro-duced in such long period, the total positive financial effect is about 8.000.000 €. The presented methodology of the reparatory hard-facing, as well as the welding pro-cedure, can be applicable, with necessary adjustments, for recovery of other parts and structures of the bucket wheel excavator at open pit mines.en_US
dc.language.isoen_USen_US
dc.publisherFaculty of Engineering University of Kragujevacen_US
dc.rightsinfo:eu-repo/semantics/openAccess-
dc.rights.urihttp://creativecommons.org/licenses/by-nc-nd/3.0/us/*
dc.source9th International Scientific Conference - IRMES 2019 - Research and Development of Mechanical Elements and Systems, Kragujevac, 2019en_US
dc.subjectReparationen_US
dc.subjectsurface weldingen_US
dc.subjectfractureen_US
dc.subjecttoothen_US
dc.subjectbucket-wheel excavatoren_US
dc.subjectgirth gearen_US
dc.titleReparatory surface welding of the fractured tooth of the bucket‐wheel excavator girth gearen_US
dc.typeconferenceObjecten_US
dc.description.versionPublisheden_US
dc.type.versionPublishedVersionen_US
Appears in Collections:Faculty of Engineering, Kragujevac

Page views(s)

212

Downloads(s)

5

Files in This Item:
File Description SizeFormat 
1212.pdf2.51 MBAdobe PDFThumbnail
View/Open


This item is licensed under a Creative Commons License Creative Commons