Please use this identifier to cite or link to this item: https://scidar.kg.ac.rs/handle/123456789/8459
Full metadata record
DC FieldValueLanguage
dc.rights.licenseopenAccess-
dc.contributor.authorVasic M.-
dc.contributor.authorKalezić-Glišović, Aleksandra-
dc.contributor.authorMilincic R.-
dc.contributor.authorRadović L.-
dc.contributor.authorMinic D.-
dc.contributor.authorMaričič A.-
dc.contributor.authorMinic D.-
dc.date.accessioned2020-09-19T15:49:04Z-
dc.date.available2020-09-19T15:49:04Z-
dc.date.issued2019-
dc.identifier.issn1450-5339-
dc.identifier.urihttps://scidar.kg.ac.rs/handle/123456789/8459-
dc.description.abstract© 2019, Journal of Mining and Metallurgy. Mehanicka aktivacija Ni 85.8 Fe 10.6 Cu 2.2 W 1.4 praškaste smeše, u vremenskim intervalima od 30-210 min, u kombinaciji sa termickom obradom na temperaturama u rasponu od 393-873 K, dovela je do mikro strukturnih promena, stvarajuci nanostrukturnu smešu istog sastva, ali sa poboljšanim magnetnim osobinama. Najbolji rezultat je ostvaren za mehanicku aktivaciju u trajanju od 120 min, prilikom termicke obrade na temperaturama oko Kirijeve tacke (693K), kada je specificna magnetizacija pocetne smeše povecana za 57%. Mikrostrukturne promene, koje obuhvataju strukturnu relaksaciju, smanjenje slobodne zapremine, gustine dislokacije i mikronaprezanja, dovode do poboljšanja strukturnih osobina materijala, i na taj nacin omogucuju bolju pokretljivost zidova magnetnih domena, kao i njihovo usmeravanje u primenjenom magnetnom polju, samim tim doprinose boljoj specificnoj magnetizaciji materijala. Sa dužim mlevenjem, veci stres akumuliran u uzorku podložniji je oslobadanju, pri cemu se procesi oslobadanja stresa pomeraju ka nižim temperaturama.-
dc.rightsinfo:eu-repo/semantics/openAccess-
dc.rights.urihttps://creativecommons.org/licenses/by-nc-nd/4.0/-
dc.sourceJournal of Mining and Metallurgy, Section B: Metallurgy-
dc.titleInfluence of mechanical activation and heat treatment on magnetic properties of nano structured mixture Ni <inf>85.8</inf> Fe <inf>10.6</inf> Cu <inf>2.2</inf> W <inf>1.4</inf>-
dc.typearticle-
dc.identifier.doi10.2298/JMMB180809004V-
dc.identifier.scopus2-s2.0-85064173051-
Appears in Collections:Faculty of Technical Sciences, Čačak

Page views(s)

452

Downloads(s)

14

Files in This Item:
File Description SizeFormat 
10.2298-JMMB180809004V.pdf4.46 MBAdobe PDFThumbnail
View/Open


This item is licensed under a Creative Commons License Creative Commons