Please use this identifier to cite or link to this item: https://scidar.kg.ac.rs/handle/123456789/12110
Title: Synthesis, structure and properties of nickel-iron-tungsten alloy electrodeposits part I: Effect of synthesis parameters on chemical Composition, Microstructure and Morphology
Authors: Ćirović N.
Spasojević P.
Ribic-Zelenovic, Lenka
Mašković, Pavle
Spasojevic M.
Issue Date: 2015
Abstract: © 2015 International Institute for the Science of Sintering (IISS). All rights reserved. Kinetic and operational electrolysis parameters determine the polarization characteristics, electrodeposition current efficiency, morphology, chemical composition and microstructure of nickel/iron/tungsten alloy deposits. The alloys electrodeposited at a current density of 50 mAcm-2 to 1000 mAcm-2 contain an amorphous phase and nanocrystals of an FCC solid solution of iron and tungsten in nickel. During annealing at temperatures above 500ºC, amorphous phase crystallization, crystalline grain growth of the FCC phase and a reduction in both internal microstrain and minimum density of chaotically distributed dislocations take place in the alloy. Milling the spongy deposit of the alloy causes amorphous phase crystallization, FCC-phase crystalline grain growth, and size reduction and rounding of powder particles.
URI: https://scidar.kg.ac.rs/handle/123456789/12110
Type: article
DOI: 10.2298/SOS1503347C
ISSN: 0350-820X
SCOPUS: 2-s2.0-84955450472
Appears in Collections:Faculty of Agronomy, Čačak

Page views(s)

533

Downloads(s)

13

Files in This Item:
File Description SizeFormat 
0350-820X1503347C.pdf1.34 MBAdobe PDFThumbnail
View/Open


This item is licensed under a Creative Commons License Creative Commons